Atmospheric plasma cleaning of glass is a solvent-free process that removes organic and carbon nano-contamination and creates hydroxyl groups for coating, bonding and lamination. One second of ROPLASS DCSBD air plasma restores complete wetting of float soda-lime glass and reduces surface carbon from 15 to 4 at.%. In a comparison of four atmospheric plasma sources, DCSBD alone met all industrial criteria for float-glass cleaning and activation.
DCSBD treats float, soda-lime, borosilicate, FTO- and ITO-coated glass as well as laminated safety-glass interlayers. In laminated safety glass, DCSBD-treated interlayers improved foil-to-glass adhesion under ball-drop testing, verified with POLARTHERM FLACHGLAS and INNOVENT e.V. (Germany) [Homola et al., NANOCON Conf. Proc., 2019]. With a UV-curing acrylate adhesive, plasma pre-treatment increased glass bond strength by more than 45% [Buček et al., International Journal of Adhesion & Adhesives 78, 2017]. Comparable results are reported on float soda-lime glass [Sihelník et al., Surfaces and Interfaces 40, 2023], on photovoltaic FTO glass [Hvojnik et al., Materials Science in Semiconductor Processing 131, 2021] and, using a linear DCSBD N₂ plasma jet, on temperature-sensitive ionoplast interlayers [Feng et al., Applied Surface Science 727, 2026].
Frequently Asked Questions
How to remove organic contamination from float glass before coating? One second of DCSBD air plasma removes organic contamination from float soda-lime glass and restores complete wetting, with the water contact angle below the detection limit. XPS shows surface carbon falling from 15 to 4 at.%; the residue is adventitious carbon re-adsorbed from air before measurement.
[Homola et al. 2013; Sihelník et al. 2023]
How to remove nanocontaminants from a glass surface? Atmospheric DCSBD plasma oxidises and desorbs adsorbed carbon nanocontaminants while forming hydroxyl groups, restoring a fully wettable surface (complete wetting). In a comparison of four atmospheric plasma sources, DCSBD alone met all industrial criteria for float-glass cleaning and activation.
[Sihelník et al. 2023]
What surface treatment improves safety glass lamination adhesion? DCSBD plasma treatment of both the glass and the interlayer before lamination improves adhesion: activation of SentryGlas ionoplast interlayer is published, and on glass the plasma raised UV-acrylate adhesive bond strength by more than 45%. Both sides of the laminate can be treated in one pass.
[Feng et al. 2025 (ionoplast); Bučék et al. 2017]
Does plasma treatment improve coating and ink adhesion on glass? Yes. Plasma-cleaned glass wets completely, so coatings and inks spread uniformly and bond to a contamination-free, hydroxylated surface. With a UV-curing acrylate adhesive, DCSBD pre-treatment increased glass bond strength by more than 45%.
[Bučék et al. 2017]
What glass types can DCSBD plasma treat? Published DCSBD work covers float soda-lime glass, display and device glass with ITO or FTO conductive coatings, and laminated safety-glass interlayers. Any flat glass format (sheets, panels or thin-glass webs) suits the thin planar plasma layer.