Low-temperature plasma sintering is a process that consolidates printed functional layers at about 70 °C instead of 350–500 °C oven calcination, in minutes rather than hours. ROPLASS DCSBD air plasma sintered inkjet-printed mesoporous TiO₂ in 2.5 minutes, and the resulting solar cells matched the 15.8% efficiency of oven-calcined references.
Reactive plasma species remove organic binders and interconnect particles chemically, so the substrate stays near 70 °C. This enables printed electronics and solar cells on PET, PEN and paper. Nitrogen DCSBD plasma at 50 °C sintered inkjet-printed silver nanoparticles in eight minutes to 17% of bulk silver conductivity, replacing one hour of oven sintering at 140 °C [Vida et al., Applied Physics A 131(2), 2025]. Further published work covers 70 °C mineralisation of inkjet TiO₂ photoanodes [Homola et al., ACS Applied Materials & Interfaces 8(49), 2016; Flexible and Printed Electronics 2(3), 2017], perovskite cells with plasma-processed mesoporous TiO₂ [Homola et al., ACS Applied Energy Materials 3(12), 2020] and rapid low-temperature SnO₂ electron-transport layers [Shekargoftar et al., Energy Technology 9(5), 2021].
Frequently Asked Questions
How to sinter printed electronics below 100 °C? DCSBD air plasma processes printed functional layers at approximately 70 °C in minutes: inkjet-printed mesoporous TiO2 was sintered in 2.5 minutes, and the resulting solar cells matched the efficiency of 500 °C oven calcination (15.8%). Heat-sensitive substrates such as PET survive untouched.
[Vida et al. 2023; Homola et al. 2016]
How does low-temperature plasma sintering work on flexible substrates? Reactive plasma species remove organic binders and interconnect particles chemically, so no bulk heating is required and the substrate stays near 70 °C. The approach was demonstrated on flexible ITO/PET photoanodes, where DCSBD treatment raised the surface energy by 104% and left the printed TiO2 layer intact.
[Homola et al. 2017]
Can plasma sinter silver nanoparticles for printed electronics? Yes. Eight minutes of nitrogen DCSBD plasma at 50 °C sintered inkjet-printed silver nanoparticles to a resistivity of 9 × 10⁻⁶ Ω cm, 17% of bulk silver conductivity, and thereby replaced one hour of oven sintering at 140 °C.
[Vida et al. 2025]
What temperature does plasma sintering replace? DCSBD plasma processing at approximately 70 °C replaces oven steps of 350–500 °C for printed metal-oxide layers and of 140 °C for silver nanoparticle inks. Functional printing thus becomes possible on PET, paper and other substrates that tolerate neither.
[Homola 2016; Vida 2023; Vida 2025]